Stainless Steel AISI 302/304
General Information
AISI 302 and 304 balls are for applications where material toughness and resistance to corrosion are more important than hardness. They have good corrosion resistance to the food environment, oxidizing solutions and most organic chemicals. Applications are valves, aerosol and finger pumps. Corrosion resistance is higher after annealing and passivation. Not resistant to sulphuric acids.
International Equivalents
DIN X5 CR Ni 18.09, AFN Z6 CN 18.09, EN58E, JIS SUS 304 Wks 1.4301
Material Specification
| Composition |
302 |
304 |
| C |
0.15 % Max |
0.08 % Max |
| Cr |
17 - 19 % |
18 - 20 % |
| Ni |
8 - 10 % |
8 - 10 % |
| Si |
1.0 % Max |
1.0 % Max |
| Mo |
1.0 % Max |
- |
| Mn |
2.0 % Max |
2.0 % Max |
| P |
0.045 % Max |
0.045 % Max |
| S |
0.03 % Max |
0.03 % Max |
(Annealed hardness on request)
| Mechanical Properties |
| Tensile Strength |
100,000 - 180,000 psi |
| Yield Strength |
50,000 - 150,000 psi |
| Density |
0.286 lbs/cu in |
If you are unsure if this is the correct material for your application, please see our Material Comparison Chart.